Cookson Group Plaskon® SMT-B-2FP Molding Compound for PBGA and CSP
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: This material is an epoxy molding compound for high temperature, lead-free reflow in fine pitch applications. It is designed to withstand more demanding requirements in moisture performance, occasioned by the higher IR reflow temperatures required for processing lead-free packages. It is a highly filled, multifunctional resin designed to pass JEDEC Level 3 at 240°C IR reflow temperatures. Features: - Lower moisture pickup
- Excellent moldability
- Low wire sweep
- Fast cure
Information provided by Cookson Electronics
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Viscosity
- Spiral Flow
- Ash
- Storage Temperature
- Hardness, Shore D
- Flexural Modulus
- Flexural Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Glass Temperature
- Flammability, UL94
- Mold Temperature
- Back Pressure
- Cure Time
- Cure Time
- Gel Time
- Shelf Life
- Hydrolyzable Halides
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|