MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Cookson Group Plaskon® CMU-870-2B Molded Underfill Compound for Flip Chip BGAs and CSPs

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:
This material is an epoxy Molded Underfill compound developed for transfer mold equipment to underfill, and overmold if needed, Flip Chip in Package (FC-BGA and FC CSP) in one step. It offers high productivity with an automated, simple, robust and fast process compared to liquid encapsulation. Higher reliability is demonstrated with the material’s higher Tg, lower CTE, no particle segregation or settling and longer outlife compared to liquid encapsulants. PLASKON CMU Series is the total molded underfill solution for Flip Chip in Package.

Features:

  • Higher productivity
  • Higher Tg
  • Higher reliability
  • Lower warpage
  • Lower CTE
  • Lower cost of ownership
  • Minimum 220°C reflow
  • Minimum JEDEC Level 3

Applications:

Plaskon CMU-870-2B Molded Underfill is suitable for high volume underfill and overmold protection of Flip Chip BGA and CSP packages. It is suitable for stack die packages using a combination of wirebonded and flip chip dies wh

Available Properties
  • Specific Gravity
  • Viscosity
  • Linear Mold Shrinkage
  • Spiral Flow
  • Ash
  • Storage Temperature
  • Hardness, Shore D
  • Flexural Modulus
  • Flexural Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Glass Temperature
  • Flammability, UL94
  • Mold Temperature
  • Back Pressure
  • Cure Time
  • Gel Time
  • Shelf Life
  • Hydrolyzable Halides
  • Preform Temperature
  • Transfer Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。