PlastxWorld CEVIAN® A1500 PA/ABS Alloy, Conditioned
Subcategory: Nylon; ABS Polymer; Thermoplastic
Key Words: Polyamide + Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Property data is for samples at equilibrium moisture (2.0%) Information provided by PlastxWorld Inc.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|