PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, Conditioned
Subcategory: Nylon; ABS Polymer; Thermoplastic
Key Words: Polyamide + Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Property data is for samples at equilibrium moisture (1.1%) These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |