PlastxWorld CEVIAN® B5523 15% GF PBT/ABS Alloy
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Glass fiber reinforced and flame retarded PBT/ABS alloy. Information provided by PlastxWorld Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|