PlastxWorld CEVIAN® SKG20 20% GF ABS
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Glass fiber reinforced, heat resistant and flame retarded ABS. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|