Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in large area broad span applications where high modulus values are required and retained. Standard processing techniques are applicable. Information provided by The Plastics Group.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Break
- Flexural Modulus
- Izod Impact, Unnotched
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|