Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuous temperature. Other benefits include reduced distortion under long-term stress. Applications: - Appliances
- Electrical components
- Automotive
- Utility products
Standard processing techniques are applicable. Information provided by The Plastics Group.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Break
- Flexural Modulus
- Flexural Strength
- Gardner Impact
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|