Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in industrial clamp components as well as bearings. Standard processing techniques are applicable. Information provided by The Plastics Group.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|