Plastics Group Polifil® 82MR Mineral-Reinforced Nylon 6 (DAM)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Polifil® GFN/MRN 6 reinforced series of compounds provide good heat and dimensional stability and offer extended or continuous stability under high temperatures. These have been found useful in industrial clamp components as well as bearings. Standard processing techniques are applicable. Information provided by The Plastics Group.
| Available Properties |
- Density
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |