Polimersan POLIKES® (PA 6 G) Cast Polyamide

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Material Notes:
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high, whereas corrosion coefficient is low. But, because of its water absorption property, it is not recommended at humid environments(%6-7).

PROPERTIES OF POLIKES®:

  • 100°C Service Temperature
  • Low Corrosion Coefficient
  • Very High Pressing Resistance
  • High Hardness
  • High Resistance To Strokes
  • Resistance To Heat
  • Resistance To Chemical Substances
  • Lower Water Absorption compared to PA 6
GENERAL USAGE AREAS OF POLIKES®:
  • Sledges
  • Wheels
  • Rolls
  • Gears
  • Bearings
  • Bobbins
  • Hoops
  • Corrosion Plates
  • Food Industry Parts
  • Chemical Industry Parts
  • Paper Industry Parts
  • Textile Industry Parts
  • Press Industry Parts

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Rockwell M
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Strength
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。