Polimersan POLIPA® (PA 6) Polyamide

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Material Notes:
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main structural key carbon atoms, which polyamide contains. Polyamide 66 contains six carbon atoms of d-amine (Hexamethylene d-amine) and six carbon atoms of d-carbonic acid (Adipinacid). This situation is valid also for polyamide 610, which is produced from hexamethyelene d-amine and sabazine acid.

Its composition has significant effect on polyamide properties. Especially, water absorption is mostly affected. As much as CH2-group exists at each CONH-group, water absorption is that much low and dimension accuracy is that very good. (1% humidity absorption equals to 0,3% length elongation.) Parts which are requested to have dimension accuracy at humid atmosphere, are full only with 1.5% water and preferably are made of polyamide 11.(For comparison this value is 10% for PA6.)

Polyamide is preferred as construction material at the conditions where exact measurements are required and which are mechanically loaded like gear wheel, rod, and bolt. Its mechanical properties are significantly dependent on its humidity quantity and degree of crystallization. It can be used also at higher temperatures because of its crystal structure and high melting point. But, when the temperature is higher than 100°C and when there is oxygen at the environment, damage occurs with oxidation. For this reason, for usage at atmosphere only stabilized ones are chosen.

As a result, POLIPA, is a hard plastic due to its high molecular weight and its structure of crosswise bonds. It is resistant to twisting and corrosion. It has the property of working for a long time under load. But, due to its water absorption (9-10%), it is not recommended at humid environments.

CHARACTERISTICS OF POLIPA®:

  • High Mechanical Resistance
  • Hardness and stroke absorption characteristic
  • Electrical Insulation
  • Sliding and high corrosion resistance
  • Resistance to chemicals
GENERAL USAGE AREAS OF POLIPA®:
  • Items which are exposed to loads with strokes
  • Gears
  • Bobbins
  • Vibration Sucking Elements
  • Engineering and maintenance applications with general purpose.

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Rockwell M
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Strength
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。