Polymer Industries Densetec HDPE Sheet
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Polymer Industry`s Densetec High Density Polyethylene sheet exhibits the properties of high impact strength, abrasion resistance, and low coefficient of friction. The material is also moisture, stain and odor resistant, and is FDA approved to be used in the food processing industry. The material`s durability makes it ideally suited for a variety of applications such as water tanks, chute linings and numerous industrial uses.Information provided by Polymer Industries.
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- CTE, linear 68°F
- Brittleness Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|