Polymer Industries Densetec HDPE Cutting Board

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Densetec Cutting Board is engineered for durability, low maintenance and safety. Its textured, matte surface safely holds food in place without slipping. The "natural" bright white color is favored for its sanitary look. Knives stay sharp when cutting on Densetec Cutting Board. Instead of striking a rigid surface that dulls the blade, Densetec Cutting Board gives on contact. Because of its unique molecular structure, cuts seal and become indiscernible.

Information provided by Polymer Industries.

Available Properties
  • Density
  • ESCR 100% Igepal®
  • Melt Index of Compound
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • CTE, linear 68°F
  • Brittleness Temperature
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。