Polymer Industries Densetec HDPE Sign Board
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Densetec Sign Board is a coextruded thermoplastic sheet with multiple color layers. The material is manufactured by extruding one color on the inside and a contrasting color on the outside. The layers are combined while the material is still molten. The result is a homogenous sheet that is guaranteed not to delaminate, crack or chip. It is superior to other sign materials, which are separate layers of material laminated together.Information provided by Polymer Industries.
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- CTE, linear 68°F
- Brittleness Temperature
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|