Polymer Industries Densetec HMW Sheet
Subcategory: Polyethylene; Thermoplastic
Material Notes: Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is more abrasion resistant. The fact that Densetec HMW is more moisture resistant and wear resistant than standard HDPE, and is more economical than standard UHMW makes it the ideal material for wear applications and machined parts. It may also be used in applications such as snowplow linings and fertilizer spreaders.Information provided by Polymer Industries.
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|