|   PolyPlastics Duranex® 733LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled  Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer Material Notes: DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives.  Therefore, as grades can be optimally designed depending on the application, various grades are provided, including flame-retardant grades, reinforced grades, and impact-resistant grades.
 DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts.  Not only does it have well-balanced properties as a raw material, DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value. Information provided by PolyPlastics. 
| | 
    | Available Properties |  
    | DensityFiller ContentTensile Strength, UltimateElongation at BreakFlexural ModulusFlexural StrengthCharpy Impact, NotchedVolume ResistivitySurface ResistanceDielectric StrengthCTE, linear 20°CCTE, linear 20°C Transverse to FlowDeflection Temperature at 1.8 MPa (264 psi)Flammability, UL94
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |