Compuestos Dominicanos polycom VN-050485 PVC
Subcategory: Vinyl; Thermoplastic
Material Notes: Description: Compuestos Dominicanos manufactures the polycom VN products for the extrusion printable sheets and banners having remarkable printing quality. Application: Sheet and banners Appearance: Natural Pellets Information provided by Compuestos Dominicanos, S.A.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
|
|
|
|