Compuestos Dominicanos polycom BD-330699 PVC
Subcategory: Vinyl; Thermoplastic
Material Notes: Description: The polycom BD series are compounds for the blow molding of PVC bottles suitable for the packing of edible oil, water, cleansing products and lubricants. These compounds produce bottles with high clarity and gloss, excellent dimensional stability and high impact resistance. Compuestos Dominicanos manufactures compounds for the blow molding of bottles up to five gallon capacity. Polycom clear products are available in violet tones dark and clear, and Compuestos Dominicanos also offers opaque products in a variety of colors. Application: Up to 1 gallon bottles Appearance: Clear light violet pellets Information provided by Compuestos Dominicanos, S.A.
| Available Properties |
- Specific Gravity
- Tensile Strength @ Break
- Izod Impact, Unnotched
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|