Polyram Bondyram 4001, Maleic Anhydride modified LLDPE coupling agent
Subcategory: Polyethylene; Additive/Filler for Polymer; Thermoplastic; LLDPE
Material Notes: Maleic Anhydride grafted linear low density polyethylene recommended as a coupling agent in PE composites with minerals and wood and compatibilizer in PE/PA blends Information provided by Polyram Ram On Ind.
| Available Properties |
- Density
- Melt Flow
- Vicat Softening Point
- Maleic Anhydride Level
|
|
|
|