Polyram Polytron Nylon 66 A50B02, Chemically Coupled 50% Long Fiber
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes: A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION Information provided by Polyram Ram On Ind.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|