Chevron Phillips Marlex® AHN-230 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Note: 2002 - This product is no longer a part of the manufacturers product line.
Material Notes: Heat stabilized, nucleated, high impact grade. All physical property testing performed on injection molded specimens.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|