Close Analogs: Note: 2002 - This product is no longer a part of the manufacturers product line.
Material Notes: General Purpose Homopolymer. All physical property testing performed on injection molded specimens.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|