Precision Polymer Engineering Perlast® G70K Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Key Words: Rubbers
Material Notes: Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended for use against strong oxidizing agents. Do not use any Perlast ® grade with molten alkali metals.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 100% Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|