Precision Polymer Engineering Perlast® G92A Perfluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Key Words: Rubbers
Material Notes: An electrically conductive black perfluoroelastomer with excellent chemical and steam resistance.Applications: Specially formulated for applications requiring special electrical properties. Originally designed for “Microfluidics” and “Lab on a Chip” applications, this material possesses good resistance to reagents and solvents whilst providing protection against static electricity build up. It has no capacitance, and a volume resistivity circa 200 ohm/cm. Do not use any Perlast ® grade with molten alkali metals.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 50% Modulus
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|