Precision Polymer Engineering Perlast® G75B High Temperature Perfluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Key Words: Rubbers

Material Notes:
Perlast® G75B offers a unique blend of excellent chemical resistance, temperature capabilities and mechanical properties, simultaneously extending the operating limits in all three aspects. Perlast® G75B has been specially formulated to provide increased acid resistance by eliminating fillers that are prone to acid attack and optimising the polymer structure. In addition, this perfluoroelastomer has low permeability and as a result, it is less prone to swelling, leading to extended in-service performance in, for example, valves, pumps and mechanical seals. A high modulus makes G75B resistant to extrusion and ideal for use in high pressure environments. In addition, the low long-term compression set provides a high mean-time between maintenance cycles in hot chemically aggressive environments. Perlast® G75B is suitable for both dynamic and static applications and can be moulded into O-rings and custom shapes.

Applications: Aerospace: Inter-stage seal assemblies (static O-rings). Chemical Processing: Pumps; Valves; Mechanical seals. Diesel: Cylinder bore liners (static O-rings); Exhaust valve seats. Semiconductor: Gas abatement systems (static); High vibration environments. Oil & Gas: High temperature down-hole environments; Electrical bulkhead feed-throughs.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • Compression Set
  • CTE, linear 20°C
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。