Precision Polymer Engineering H70B Epichlorohydrin
Subcategory: Elastomer, TS; Thermoset
Material Notes: Peroxide Cured, Epichlorohydrin Rubber, 65-75 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. ASTM and ISO designation = GECO.Applications: Excellent resistance to petroleum based oils and fuels. Becoming widely used in military and automotive applications where its low and high temperature operating range is superior to that of nitrile. Good resistance to water, acide, ozone and weathering.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|