Precision Polymer Engineering E70H Ethylene Propylene Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Peroxide cured, white Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title (CFR21), Section 177.2600. Extraction tested in distilled water. Also complies with the requirements of USP 25, NF20, 2002, Class 6.Applications: Excellent water and steam resistance with good compression set properties. Heat and chemical resistance is superior to that of sulphur cured EPDM. Not oil resistant.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Extraction Test, 21 CFR 177.2600
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|