Precision Polymer Engineering E80A Ethylene Propylene Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Blue, Ethylene Propylene Terpolymer (EPT), 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA), in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600. ASTM & ISO designation = EPDM.Applications: Formulated for repeated use with aqueous foodstuffs intended for human consumption. Not suitable for use with fatty foodstuffs.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|