Precision Polymer Engineering V70J Fluoroelastomer Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Grey Fluoroelastomer Rubber, 65-75 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B38, EF31, EO78, Z2, where Z2 = colour grey. ASTM designation = FKM. ISO designation = FPM.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air