Precision Polymer Engineering V71C Fluoroelastomer Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Fluoroelastomer Rubber, 66-75 °IRHD. Terpolymer of vinylidene difluoride and hexafluoropropylene tetrafluoroethylene. Compounded to have extremely low temperature capability, Glass transition temperature -40 °C. Dependant on application, use temperature can be lower than this.Applications: Mouldings which are required to operate within the approximate temperature range of -40° and below to +225°C, in contact with air, petroleum, silicone and diester-based liquids. The material is not suitable for use in contact with certain phosphate-ester-based liquids.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Glass Transition, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|