Precision Polymer Engineering V72H Fluoroelastomer Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600.Applications: Excellent oil and heat resistance combine with low compression set performance. Used primarily in food processing and pharmaceutical equipment. Excellent ozone resistance.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|