Precision Polymer Engineering V97B Fluoroelastomer Compound
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Where Z1 = hardness 90-98. ASTM designation = FKM. ISO designation = FPM.Applications: A hard, anti-extrusion resistant rubber, specially designed for use in high pressure applications. Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|