Precision Polymer Engineering F50A Fluorosilicone Rubber
Subcategory: Fluoropolymer, TS; Silicone; Elastomer, TS; Thermoset
Material Notes: Blue Fluorosilicone, 45-55 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.