Precision Polymer Engineering F60R Fluorosilicone Rubber
Subcategory: Fluoropolymer, TS; Silicone; Elastomer, TS; Thermoset
Material Notes: Red Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 60.Applications: Sealing petroleum-based fuels, hydraulic fluids and lubricants, and with silicone and certain ester-based fluids (but excluding certain phosphate esters).
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|