Precision Polymer Engineering F70A Fluorosilicone Rubber
Subcategory: Fluoropolymer, TS; Silicone; Elastomer, TS; Thermoset
Material Notes: Blue Fluorosilicone Rubber, 60 to 70 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 70.Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|