Precision Polymer Engineering F80X Fluorosilicone Rubber
Subcategory: Fluoropolymer, TS; Silicone; Elastomer, TS; Thermoset
Material Notes: Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 80.Applications: Intended for use in applications where resistance to jet fuels, hydraulic fluids, lubricants, silicone and ester-based fluids (but excluding certain phosphate esters) is required.