Precision Polymer Engineering Kemex™ V76W
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Kemex™ ETP fluoroelastomer is a premium peroxide cured fluoroelastomer that exhibits improved fluid resistance over any FKM fluoroelastomer. It is designed for severe service applications, which require chemical resistance to strong bases and amines and good resistance to polar solvents. Kemex™ is based upon ETP terpolymer and is a new generation of fluoroelastomer consisting of ethylene, tetrafluoroethylene and perfluormethylvinylether. Kemex™ bridges the gap between fluoroelastomers, Aflas® and Perlast® perfluoroelastomer. It provides the best chemical resistance of all fluoroelastomers and is available in a wide range of compounds. Kemex™ was originally developed for use in oil field applications, in contact with amines and sour oils. However, due to its excellent chemical resistance properties it is now widely used in the CPI industry due to its suitability for use with fuels with additives, spray coatings, alcohols and solvents such as toluene, ETBE and MTBE.Applications: Kemex™ has been specially developed for severe applications that require a combination of heat, fluid and base resistance combined with low temperature flexibility. Applications which Kemex™ exhibits excellent resistance include: Aliphatic and aromatic hydrocarbons; Hydraulic Fluids; Motor Oils; Fuels and alcohol. Kemex™ also shows good resistance to base containing fluids and polar solvents.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|