Precision Polymer Engineering Z70F Hydrogenated NBR Compound
Subcategory: Elastomer, TS; Thermoset
Material Notes: Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations, Title 21 (CFR21), Section 177.2600 and Section 180.22. Extraction tested.Applications: High strength and excellent chemical resistance. Higher operating temperature than standard nitrile. Material designed for repeated use in equipment associated with the production of fatty and aqueous foodstuffs. Steam resistant.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Extraction Test, 21 CFR 177.2600
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|