Precision Polymer Engineering Z75G Hydrogenated NBR Compound
Subcategory: Elastomer, TS; Thermoset
Material Notes: Green Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.Applications: High strength and excellent chemical resistance. Higher operating temperature than standard nitrile. Suitable for use with sour (H2S) crude oil and gas, which may also include lubricating, oil additives and amine corrosion inhibitors. Good resistance to weathering and ozone.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|