Precision Polymer Engineering Z95X Hydrogenated NBR Compound
Subcategory: Elastomer, TS; Thermoset
Material Notes: Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applications where explosive decompression may occur. Suitable for use with sour (H2S) crude oil and gas, which may also include lubricating, oil additives and amine corrosion inhibitors. High mechanical strength and excellent chemical resistance.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|