Precision Polymer Engineering Z95Z Hydrogenated NBR Compound
Subcategory: Elastomer, TS; Thermoset
Material Notes: Peroxide cured and methacrylate modified, hydrogenated nitrile rubber, 80-92 °IRHD. Medium acrylonitrile content (ACN=36%). ASTM designation = HNBR.Applications: For uses where very high physical properties, abrasion resistance, low hysteresis and excellent flex-life are required. Where applicable, designed to withstand solutions between 3.5 to 13 pH and fluids similar to ASTM #1 oil and hot water, but also capable of maintaining physical properties at high temperatures.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|