Precision Polymer Engineering N50C Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene Rubber, 45-55 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class B, approval ref.: 67/6.11.iv. MSL lab code 1.R. Also meets British Standard BS2494 Type G.Applications: Elastomeric seals for use in pipelines carrying manufactured or natural gas at operating temperatures of -5° to +40°C and pressures up to 7 bar.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|