Precision Polymer Engineering N60N Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 60.Applications: Synthetic rubber resistant to petroleum-based fuels and diester-based lubricants. They are unsuitable for use in contact with phosphate ester hydraulic fluids and have poor ozone resistance.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|