Precision Polymer Engineering N70C Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class D, approval ref.: 31/6.1.vii. MSL lab code 2P.670. Also meets British Standard BS2494 Type G.Applications: Elastomeric seals for use in pipelines carrying manufactured or natural gas at operating temperatures of -5°C to +40°C and pressures up to 7 bar.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|