Precision Polymer Engineering N70F Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title 21 (CFR21), Section 177.2600 and Section 180.22. Water, Hexane and acrylonitrile extraction tested. Tested to 3A requirements.Applications: Repeated use in equipment associated with the production of foodstuffs intended for human consumption.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Extraction Test, 21 CFR 177.2600
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|