Precision Polymer Engineering N70M Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene Rubber (NBR), 68-78 °IRHD. Copolymer of acrylonitrile and butadiene. To meet BS2751 BA70 and ASTM D2000/SAE J200 line call-out 2MBG 714, B14, EA14, EF11, EF21, EO14, EO34, F17.Applications: Excellent resistance to petroleum based oils and fuels. Excellent compression set, tear and abrasion resistance. Good water resistance, but poor against ozone and weather.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|