Precision Polymer Engineering N70V Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Nitrile Butadiene/PVC Rubber, 65-75 °IRHD. Copolymer of acrylonitrile and butadiene blended with PVC.Applications: Excellent resistance in sealing applications against petroleum and mineral based fuels and oils. Compounded with PVC to provide improved resistance to ozone and weathering.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|