Precision Polymer Engineering N90B Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: General purpose, Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM & ISO designation = NBR. ASTM D2000 line call-out: M4CH910, A25, B14, EF31, EO15, EO35, F16.Applications: Excellent resistance to petroleum based oils and fuels. Excellent compression set, tear and abrasion resistance. Good water resistance but poor against ozone and weather.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|