Precision Polymer Engineering N90K Nitrile Rubber
Subcategory: Elastomer, TS; Thermoset
Material Notes: Peroxide cured Nitrile Rubber, 85-95 °IRHD. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. ASTM D2000/SAE J200 line call-out M7BG910, B14, EA14, EF11, EF21, EO14, EO34, F16.Applications: Excellent resistance in sealing applications for petroleum based oils and fuels. Excellent compression set, tear and abrasion resistance. Good water resistance but poor against ozone and weather.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Compression Set
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Low Temperature Resistance, °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|